MMO Tubular Anode
MMO tubular anodes can be used directly in freshwater or seawater environments. For large offshore steelstructure cathodic protection, they can be assembled into remote ground anodes with simple installation and wide protection range. In soil conditions, prepackaged MMO tubular anodes form shallowburied or deepwell anode ground beds.
Prepackaged MMO Anode: Outer MMO tubular anode fitted with solidcopper terminal for good conductivity, connected with special YJV or PVDF/HMWPE cables. Filled with coke particles for maximum surface current output and sealed by epoxy resin. Multiple units can be connected in series or parallel to build complete prepackaged anode groups.
Specifications & Performance
| Item | OD (mm) | Wall Thickness (mm) | Length (mm) | Surface Area (㎡) | Current Output (mA/m) | Service Life (Years) |
| Tubular Anode | 16 | 1.0 | 1000 | 0.05 | 5 | 2030 |
| 16 | 1.0 | 1000 | 0.05 | 30 | 2030 | |
| 19 | 1.0 | 1000 | 0.06 | 6 | 2030 | |
| 19 | 1.0 | 1000 | 0.06 | 36 | 2030 | |
| 25 | 1.0 | 1000 | 0.08 | 8 | 2030 | |
| 25 | 1.0 | 1000 | 0.08 | 48 | 2030 | |
| 32 | 1.0 | 1000 | 0.10 | 10 | 2030 | |
| 32 | 1.0 | 1000 | 0.10 | 60 | 2030 |
Custom dimensions available upon request Coating system: RutheniumIridium / IridiumTantalum Titanium substrate standard: ASTM B338 Gr1 titanium tube
Chemical Composition (Max. wt%)
| Fe | C | N | H | O | Ti | Others |
| 0.20% | 0.08% | 0.03% | 0.02% | 0.18% | Balance | 0.40% |
Accelerated life test standard: NACE TM01082008
| Coating System | Medium | Current Density(A/㎡) | Temperature(℃) |
| IridiumTantalum | 1 mol/L Na₂SO₄ | 20000 | 40±5 |